Latest Patents

Patents imply intellectual property and it has a $ value that can be associated depending on the field and type of patent that is allocated. Patents also increase the enterprise value of the company and help prevent copy-cats from copying the idea without having royalt payments or licencing deals. We like it when companies get patents awarded!. To protect IP companies aggressively file provisional patents even before they have a working product. The below table provides a way to look at what has been done by companies and use this as a factor to make investment decisions.

     
Title Filing Date Publication Date Grant Date
Wroughtable, chromium-bearing, cobalt-based alloys with improved resistance to … 2022-11-11 2023-1-01
Cobalt-chromium alloy resistant to high speed/self-coupling sliding wear 2022-3-24 2022-9-30
Solar tower system containing molten chloride salts (divisional from … 2021-11-26 2022-7-22
Fabricable, High Strength, Oxidation Resistant Ni-Cr-Co-Mo-Al Alloys 2019-6-27 2019-10-24
HEAT TREATMENTS FOR IMPROVED DUCTILITY OF Ni-Cr-Co-Mo-Ti-Al ALLOYS. 2018-11-09 2020-11-11
NI-CR-MO ALLOYS and method for producing same 2016-7-08 2017-1-18
Acid and alkali resistant nickel-chromium-molybdenum-copper alloys 2016-6-09 2016-10-06
Acid and Alkali Resistant Ni-Cr-Mo-Cu Alloys with Critical Contents of Chromium … 2016-6-09 2016-10-06
acid and alkali resistant ni-cr-cu-alloys with critical chromium and copper … 2013-11-08 2015-10-27
Acid And Alkali Resistant Ni-cr-mo-cu Alloys With Critical Contents Of Chromium … 2013-10-30 2014-6-25
Acid and alkali resistant nickel-chromium-molybdenum-copper alloys 2013-10-29 2015-5-14
Acid and alkali resistant ni-cr-mo-cu alloys with critical contents of chromium … 2013-10-29 2015-4-29
Nickel-chrome-molybdenum-copper alloy having acid resistance and alkaline … 2013-10-29 2015-4-23
Acid alkali resistant ni-cr-mo-cu alloys with critical contents of chromium and … 2013-10-29 2014-7-30
Acid and alkali resistant Ni-Cr-Mo-Cu alloys with critical chromium and copper … 2013-10-25 2020-3-16 2020-3-16
Weldable oxidation resistant nickel-iron-chromium aluminum alloy 2013-7-12 2013-11-07
Acid and alkali resistant nickel-chromium-molybdenum-copper alloys 2013-4-30 2013-12-16
Mold having ceramic insert 2012-8-30 2014-3-06
High temperature low thermal expansion Ni-Mo-Cr alloy 2012-2-17 2013-10-01 2013-10-01
AGING TREATMENT FOR Ni-Cr-Mo ALLOY 2010-7-09 2010-11-25
Weldable oxidation resistant nickel-iron-chromium-aluminum alloy 2008-12-12 2009-6-17
Cobalt-chromium-iron-nickel alloys amenable to nitride strengthening 2007-9-14 2008-4-03
Hybrid corrosion-resistant nickel alloy 2007-8-08 2008-2-21
Hybrid corrosion-resistant nickel alloys 2007-8-08 2008-2-13
Ni-Cr-Co Alloy for advanced gas turbine engines 2007-6-13 2008-1-03
Ni-Cr-Co alloy for advanced gas turbine engines 2006-6-13 2011-11-29 2011-11-29
Ni-cr-co alloy for advanced gas turbine engines. 2005-9-02 2006-3-07
Ni-cr-mo alloys having improved corrosion resistance 2004-12-09 2006-5-03
A nickel-chromium-molybdenum alloy 2004-9-03 2005-3-09
Age-Hardenable, corrosion resistant Ni-Cr-Mo Alloys 2004-9-02 2005-3-24
Sulphuric acid and wet phosphorus acid resistant Ni-Cr-Mo-Cu alloy 2003-6-13 2006-10-18 2006-10-18
Nickel-chromium-molybdenum alloy resistant to local corrosion due to wet- … 2003-5-14 2004-1-08
AGING TREATMENT FOR Ni-Cr-Mo ALLOY 2002-6-28 2003-3-05
TWO-STEP AGING TREATMENT FOR Ni-Cr-Mo ALLOY 2002-6-28 2003-1-29
TWO-STAGE AGING PROCESS FOR NI-CR-MO ALLOYS 2002-6-26 2012-5-15